Seam welding is a resistance welding process in which the electrodes are rotating copper wheels. The sheets travel between the wheels while current pulses are applied, producing a row of overlapping spots that forms a continuous, leak-tight joint.
How Does Seam Welding Work?
Two wheels (or one wheel against a bar or mandrel) hold the sheets under constant force and move them forward as they rotate.
Each pulse forms one weld spot. Between pulses there is a cool time that keeps the sheet and the wheel from overheating.
Travel speed and pulse rate are set so that each spot overlaps the one before it. The result is a seam that is tight to liquids and gases.
Heat is generated as in any resistance weld (Q = I²Rt). Because the wheel works continuously, it is almost always cooled with water applied directly to the weld zone.
Types of Seam Welding
Lap seam
The two sheets overlap and are welded along the lap. The most common form in tanks and containers.
Mash seam
The overlap is very small and the wheels mash it down during welding. The joint ends up nearly flush, close to the thickness of a single sheet.
Roll spot
Pulses are spaced apart to leave separate spots instead of a continuous seam. Used where strength is needed but leak tightness is not.
Continuous or intermittent
In continuous seam welding the wheel never stops. In intermittent welding it stops at each spot: slower, but used on heavier gauges.
Where Is Seam Welding Used?
- Fuel tanks and automotive reservoirs.
- Radiators and transformer tanks.
- Drums, pails and cans.
- Water heaters and thin-wall pressure vessels.
- Mufflers and exhaust systems.
What Material Are Seam Welding Wheels Made Of?
The wheel is an electrode: it has to carry high current while resisting force and heat without deforming.
The most widely used material for seam welding wheels on carbon steel. A good balance of conductivity and hardness. See Class 2 copper.
Higher conductivity. Preferred on coated sheet or aluminum, where the wheel tends to stick. See Class 1 copper.
Higher hardness. Used where welding force is high, as with stainless steel. See Class 3 copper.
A forged wheel has a denser, more uniform grain than one cut from plate, so it wears more evenly. See our forged wheels for seam welding.
Common Problems and Their Causes
The spots are not overlapping: travel speed is too high or the pulses are too far apart.
Too much current, not enough cooling, or a wheel face contaminated with coating picked up from the sheet.
The wheel face has spread with use. The profile has to be redressed to restore the original contact width.